Test Clause |
Requirement |
Conditioning |
1) dried for at least 30 minutes at 105°C ± 3°C (220°F ± 5°F) |
2) If the specimens melt or permanently deform at 105°C (220°F) or below, the specimens shall be conditioned at 20°C ± 5°C (68°F ± 9°F) for at least 24 hours prior to flame exposure. |
|
Method 1 |
the density Less Than 700g/m2 |
Method 2 (can be folded) |
the density More Than 700g/m2 |
Method 2 (can not be folded) |
|
* Cleansing extra (if required) |
|
Sample Required: |
|
Method 1 |
10 pieces in the size of 400mmX150mm |
Method 2 (Can be folded) |
4 pieces in the size of 610mm X1200mm |
Method 2 (can not be folded) |
10 pieces in the size of 125mm X1200mm |
With the length parallel to the lengthwise direction of the material |
|
Turnaround time: normal (9 working days), |
|
所需时间: 标准(9 个工作天) |
|
Note: When a manufacturer claims that the material tested in accordance with this standard retains its flame resistance after cleaning or weathering, then need related washing or weathering procedure. |
Sample for reference 参考图片: